{"sample":{"thickness":"11 layers","processings":{"processing_steps":"The graphene layers were grown in a closed rf induction furnace at a temperature of 1550 %B0C"},"substrate_material":"SiC","comments":"","parameters_environment":{"temperature":"6"},"name":"Graphene","material":{"phase_name":"","chemical_formula":"C%2FSiC%28000-1%29","family":"2D"},"publication":{"citation":""}},"experiments":{"comments":"","variable_parameters_comments":""},"experiment":{"uid":"EXPERIMENT_2009-11-27_982502eff1fedd2cc8fd1c7b5002bb41a3788f996579e215318d78f3608d83da","publication":{"citation":"10.1103%2FPhysRevLett.103.226803"},"spectra":{"spectrum":{"reference_position":"The scan in ky is perpendicular to the SiC %3C10-10%3E direction at the K point.","analysis":""}},"date_begin":"2009-11-27","description":"","types":{"type":"laboratory measurement "},"variable_parameters_types":"temperature ","parameters_instrument":{"spectrum_scan_number":"","polarization":"","spectral":{"ranges":{"range":{"resolution":"7 meV","sampling":""}}},"spatial":{"extent_z":"","extent_x":"","extent_y":""}},"title":"Graphene on SiC%28000-1%29"},"datafiles":"Fig2_PRL_103_226803_Sprinkle.jpg;","experimentalist":{"laboratories":{"laboratory":""},"family_name":"","email":""},"user_id":"tejeda","url":"https://data-analysis.synchrotron-soleil.fr/sharpes/db/EXPERIMENT_2009-11-27_982502eff1fedd2cc8fd1c7b5002bb41a3788f996579e215318d78f3608d83da","Submit":"Submit entry","dataset":"Fig2_PRL_103_226803_Sprinkle.jpg","database":"DB_sharpes","uid":"982502eff1fedd2cc8fd1c7b5002bb41a3788f996579e215318d78f3608d83da","date":"Mon Aug 17 10:37:36 2026","instrument":{"source_power":"","technique":"ARPES","detectors":{"detector":""},"source_energy":"30","name":"","comments":"","source":"synchrotron ","spectral_analyzers":""}}